Acero bajo en carbono
EN 10028-2 Grade P355GH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10028-3 Grade P355NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10028-3 Grade P355NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Medium Carbon Steel
EN 10028-3 Grade P355N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S960Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10149-2 Grade S650MC thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10149-2 Grade S700MC thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 HT, Heat-TreatedSuministrada por:
1 proveedor Matmatch
Nickel Chromium Molybdenum Steel
Carbodur 6587 Blank HardenedSuministrada por:
Deutsche Edelstahlwerke (DEW)