Conductividad térmica: 15.3 W/(m·K)

Quick Comparison

Acero inoxidable martensítico

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Suministrada por:

1 proveedor Matmatch

Nickel Chromium Iron Alloy

VDM® Alloy 800

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy 800 H

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy 800 HP

Suministrada por:

VDM Metals

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Suministrada por:

1 proveedor Matmatch

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Acero inoxidable austenítico

UGIMA® 4305HM Solution Annealed

Suministrada por:

Ugitech

Acero inoxidable austenítico

UGIMA® 4305HM Work Hardened (drawn)

Suministrada por:

Ugitech

Acero inoxidable austenítico

UGIMA®-X 4305 Solution Annealed

Suministrada por:

Ugitech

Acero inoxidable austenítico

UGIMA®-X 4305 Cold Drawn

Suministrada por:

Ugitech
Página 1 de 149