BrewerBOND® T1107

Alternative and trade names
High performance polymer
Want to keep this datasheet? Save it now in your required format

Description

A high temperature thermoplastic solution with high glass transition temperature, high melt viscosity, sensitive to UV laser for etching or separation purposes, chemically resistant with no curing needed.

This material data has been provided by Brewer Science.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.0032 g/cm³

Show Supplier Material materials with Density of 1.0032 g/cm³

Exact value: 1.00324

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

2.9 GPa

Show Supplier Material materials with Elastic modulus of 2.9 GPa

Tensile strength

23.0 °C

85 MPa

Show Supplier Material materials with Tensile strength of 85 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.8E-5 1/K

Glass transition temperature

328 °C

Show Supplier Material materials with Glass transition temperature of 328 °C

Max service temperature

410 °C

Show Supplier Material materials with Max service temperature of 410 °C

decomposition temperature

Technological properties

Property
Application areas

High temperature adhesives and bonding