OptiStack® SOC460D

Alternative and trade names
High performance polymer
Want to keep this datasheet? Save it now in your required format

Description

spin-on thermoset material solution, with a high carbon content, high temperature thermal stability, planarization properties

This material data has been provided by Brewer Science.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyValue

Max service temperature

400 °C

Show Supplier Material materials with Max service temperature of 400 °C

Technological properties

Property
Application areas

Surface Planarization, High Temperature Gap fill, Spin-on Carbon, High temperature thermoset, Semiconductor Industry, Aerospace, Automotive, Packaging, Electronic Packaging