High performance polymer
Want to keep this datasheet? Save it now in your required format

Description

A high temperature thermoset solution with low glass transition temperature, UV and thermally curable with high thermal stability and high chemical resistance

This material data has been provided by Brewer Science.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9042 g/cm³

Show Supplier Material materials with Density of 0.9042 g/cm³

Exact value: 0.90424

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

3.3E-3 GPa

Show Supplier Material materials with Elastic modulus of 3.3E-3 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

3.9E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.9E-4 1/K

Glass transition temperature

-50 °C

Show Supplier Material materials with Glass transition temperature of -50 °C

max.

Max service temperature

350 °C

Show Supplier Material materials with Max service temperature of 350 °C

decomposition temperature

Technological properties

Property
Application areas