Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
BrewerBOND® 530
High temperature stable mechanical debond material. Polar solvent system with room temperature debonding and excellent chemical resistance.
This material data has been provided by Brewer Science.
All categories
General
Property | Value | Comment |
---|---|---|
Contact angle | 91 ° Show Supplier Material materials with Contact angle of 91 ° | with water |
Dimension
Property | Value | Comment |
---|---|---|
Thickness | 2.5E-4 mm Show Supplier Material materials with Thickness of 2.5E-4 mm | Nominal coat thickness |
Thermal
Property | Value |
---|---|
Max service temperature | 300 °C Show Supplier Material materials with Max service temperature of 300 °C |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Viscosity | 23.0 °C | 12 Pa·s Show Supplier Material materials with Viscosity of 12 Pa·s |
Technological properties
Property | ||
---|---|---|
Application areas | High temperature temporary adhesives and bonding |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2022 Matmatch GmbH, All rights reserved.
Made with ❤️ in Munich!