BrewerBOND® 701

Alternative and trade names
High preformance polymer
Want to keep this datasheet? Save it now in your required format

Description

High temperature stable laser debond material. Polar solvent system with low stress (zero force) debonding for high temperature process and ultrathin samples

This material data has been provided by Brewer Science.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Viscosity

23.0 °C

7 Pa·s

Show Supplier Material materials with Viscosity of 7 Pa·s

valueMetaData

PropertyValueComment

Thickness

1.5E-4 mm

Show Supplier Material materials with Thickness of 1.5E-4 mm

Nominal coat thickness

Thermal

PropertyValue

Max service temperature

400 °C

Show Supplier Material materials with Max service temperature of 400 °C

Technological properties

Property
Application areas

High temperature temporary adhesives and bonding