OptiStack® SOC304

Alternative and trade names
High performance polymer
Want to keep this datasheet? Save it now in your required format

Description

spin-on thermoset material solution, with a high carbon content, planarization properties

This material data has been provided by Brewer Science.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.45E-4 - 2.35E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.45E-4 - 2.35E-4 1/K

respectively for below and above Tg

Glass transition temperature

178 °C

Show Supplier Material materials with Glass transition temperature of 178 °C

Max service temperature

300 °C

Show Supplier Material materials with Max service temperature of 300 °C

Technological properties

Property
Application areas

Surface Planarization, High Temperature Gap fill, Spin-on Carbon, High temperature thermoset, Semiconductor Industry, Aerospace, Automotive, Packaging, Electronic Packaging