TECACOMP PE ID blue 3943

Alternative and trade names
PE-MD
Want to keep this datasheet? Save it now in your required format

Description

PE (Polyethylene) with mineral filler. Main features : detectable via metal detector , x-ray detectable and FDA compliant

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.26 g/cm³

Show Supplier Material materials with Density of 1.26 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.19 GPa

Show Supplier Material materials with Elastic modulus of 0.19 GPa

DIN EN ISO 527-1, 50mm/min

Elongation

23.0 °C

120 %

Show Supplier Material materials with Elongation of 120 %

DIN EN ISO 527-1, 50mm/min

Tensile strength

23.0 °C

10 MPa

Show Supplier Material materials with Tensile strength of 10 MPa

DIN EN ISO 527-1, 50mm/min

Impact strength, Charpy unnotched

No Break, DIN EN ISO 179-1eU

Thermal

PropertyValueComment

Glass transition temperature

-100 °C

Show Supplier Material materials with Glass transition temperature of -100 °C

DIN 53765

Max service temperature, long

70 °C

Show Supplier Material materials with Max service temperature, long of 70 °C

Max service temperature, short

100 °C

Show Supplier Material materials with Max service temperature, short of 100 °C

Melting point

109 °C

Show Supplier Material materials with Melting point of 109 °C

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

19 g/10min

Show Supplier Material materials with Melt mass-flow rate of 19 g/10min

DIN EN ISO 1133, 230°C/5kg

Melt volume-flow rate

18 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min

DIN EN ISO 1133, 230°C/5kg

Shrinkage

23.0 °C

3 %

Show Supplier Material materials with Shrinkage of 3 %

DIN EN ISO 294-4

Shrinkage, transverse

23.0 °C

1.84 %

Show Supplier Material materials with Shrinkage, transverse of 1.84 %

DIN EN ISO 294-4

Technological properties

Property
Certifications

FDA compliant

Color

Blue

Detectability

Inductive: 6 mm Al, X-Ray detectable: 3.5 mm Al

Fillers

Mineral Powder

Processing methods

Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 4, mould temperature (°C): 40, material temperature (°C): 240, cylinder/processing temperature (°C): 240