TECACOMP PA66 TC black 3989

Want to keep this datasheet? Save it now in your required format

Description

PA 66 (Polyamide 66) filled with graphite. Main features: high thermal conductivity , electrically conductive

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.7 g/cm³

Show Supplier Material materials with Bulk density of 0.7 g/cm³

EN ISO 60

Density

23.0 °C

1.48 g/cm³

Show Supplier Material materials with Density of 1.48 g/cm³

Water absorption

23.0 °C

1.5 %

Show Supplier Material materials with Water absorption of 1.5 %

DIN EN ISO 62, 23 °C / 50 % relative humidity up to saturation

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

8.1 GPa

Show Supplier Material materials with Elastic modulus of 8.1 GPa

DIN EN ISO 527-1, 50mm/min

Elongation

23.0 °C

1.5 %

Show Supplier Material materials with Elongation of 1.5 %

DIN EN ISO 527-1, 50mm/min

Impact strength, Charpy unnotched

23.0 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 11 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

57 MPa

Show Supplier Material materials with Tensile strength of 57 MPa

DIN EN ISO 527-1, 50mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

61.5 °C

3.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.8E-5 1/K

DIN EN ISO 11359-1;2, values applicable for the range 61.5±38.5°C, 125±25°C

125.0 °C

7.1E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7.1E-5 1/K

DIN EN ISO 11359-1;2, values applicable for the range 61.5±38.5°C, 125±25°C

Coefficient of thermal expansion, transverse

61.5 °C

4.7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.7E-5 1/K

DIN EN ISO 11359-1;2, values applicable for the range 61.5±38.5°C, 125±25°C

125.0 °C

7.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.4E-5 1/K

DIN EN ISO 11359-1;2, values applicable for the range 61.5±38.5°C, 125±25°C

Unlock all property charts

Glass transition temperature

50 °C

Show Supplier Material materials with Glass transition temperature of 50 °C

DIN 53765

Heat deflection temperature, 1.80 MPa

232 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 232 °C

ISO-R 75 Method A

Max service temperature, long

110 °C

Show Supplier Material materials with Max service temperature, long of 110 °C

Max service temperature, short

170 °C

Show Supplier Material materials with Max service temperature, short of 170 °C

Melting point

255 °C

Show Supplier Material materials with Melting point of 255 °C

DIN 53765

Specific heat capacity

23.0 °C

1500 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 1500 J/(kg·K)

DIN EN 821

Thermal conductivity, in-plane

23.0 °C

11.2 W/(m·K)

Show Supplier Material materials with Thermal conductivity, in-plane of 11.2 W/(m·K)

DIN EN 821

Thermal conductivity, through-plane

23.0 °C

2.8 W/(m·K)

Show Supplier Material materials with Thermal conductivity, through-plane of 2.8 W/(m·K)

DIN EN 821

Thermal diffusivity, in-plane

23.0 °C

5.1 mm²/s

Show Supplier Material materials with Thermal diffusivity, in-plane of 5.1 mm²/s

DIN EN 821

Thermal diffusivity, through-plane

23.0 °C

1.3 mm²/s

Show Supplier Material materials with Thermal diffusivity, through-plane of 1.3 mm²/s

DIN EN 821

Flammability

UL94 class HB, DIN IEC 60695-11-10

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

10000 Ω/sq

Show Supplier Material materials with Surface resistivity of 10000 Ω/sq

max., DIN EN 61340-2-3

Volume resistivity

23.0 °C

3500 - 10000 Ω·cm

Show Supplier Material materials with Volume resistivity of 3500 - 10000 Ω·cm

respectively for DIN EN ISO 3915, DIN EN 61340-2-3

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

36 g/10min

Show Supplier Material materials with Melt mass-flow rate of 36 g/10min

DIN EN ISO 1133, 230°C/2.16kg

Shrinkage

23.0 °C

0.78 %

Show Supplier Material materials with Shrinkage of 0.78 %

DIN EN ISO 294-4

Shrinkage, transverse

23.0 °C

1.02 %

Show Supplier Material materials with Shrinkage, transverse of 1.02 %

DIN EN ISO 294-4

Technological properties

Property
Application areas

Electrical engineering , Mechanical engineering , Automotive industry

camera, moulded interconnect device (PCB, LDS), power distribution in electronics and radar

Color

Black

Detectability

Fillers

Graphite

Processing methods

Drying temperature (°C): 80, drying time (h): 5, mould temperature (°C): 150, material temperature (°C): , cylinder/processing temperature (°C): 295