TECACOMP PE ID black 1054878 no datasheet

Alternative and trade names
PE-MD
Want to keep this datasheet? Save it now in your required format

Description

PE (Polyethylene) with detectable filler. Main features: detectable via metal detector, x-ray detectable and Explanation of food contact according to FDA and EU 10/2011 on request

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

1.11 g/cm³

Show Supplier Material materials with Bulk density of 1.11 g/cm³

EN ISO 60

Density

23.0 °C

2.38 g/cm³

Show Supplier Material materials with Density of 2.38 g/cm³

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

max., DIN EN ISO 62, 23 °C / 50 % relative humidity up to saturation

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.91 GPa

Show Supplier Material materials with Elastic modulus of 0.91 GPa

DIN EN ISO 527-1

Elongation

23.0 °C

12 %

Show Supplier Material materials with Elongation of 12 %

DIN EN ISO 527-1

Flexural modulus

23.0 °C

0.6 GPa

Show Supplier Material materials with Flexural modulus of 0.6 GPa

DIN EN ISO 178

Flexural strain

23.0 °C

12 %

Show Supplier Material materials with Flexural strain of 12 %

DIN EN ISO 178

Flexural strength

23.0 °C

20 MPa

Show Supplier Material materials with Flexural strength of 20 MPa

DIN EN ISO 178

Impact strength, Charpy unnotched

23.0 °C

60 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

14 MPa

Show Supplier Material materials with Tensile strength of 14 MPa

DIN EN ISO 527-1

Thermal

PropertyValueComment

Glass transition temperature

-100 °C

Show Supplier Material materials with Glass transition temperature of -100 °C

DIN 53765

Max service temperature, long

70 °C

Show Supplier Material materials with Max service temperature, long of 70 °C

Max service temperature, short

100 °C

Show Supplier Material materials with Max service temperature, short of 100 °C

Melting point

109 °C

Show Supplier Material materials with Melting point of 109 °C

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

12.4 g/10min

Show Supplier Material materials with Melt mass-flow rate of 12.4 g/10min

DIN EN ISO 1133, 230°C /5kg

Melt volume-flow rate

6.1 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 6.1 cm³/10min

DIN EN ISO 1133

Shrinkage

23.0 °C

1.67 %

Show Supplier Material materials with Shrinkage of 1.67 %

DIN EN ISO 294-4

Shrinkage, transverse

23.0 °C

1.6 %

Show Supplier Material materials with Shrinkage, transverse of 1.6 %

DIN EN ISO 294-4

Technological properties

Property
Certifications

Explanation of food contact according to FDA and EU 10/2011 on request

Color

Black

Fillers

Detectable Filler

Processing methods

Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 44231, mould temperature (°C): 30-60, material temperature (°C): 200-240, cylinder/processing temperature (°C): 190-240