TECACOMP PPA TRM XS mod. black 1054920

Want to keep this datasheet? Save it now in your required format

Description

PPA (Polyphtalamide) with good slide and wear properties

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.25 g/cm³

Show Supplier Material materials with Density of 1.25 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

15 GPa

Show Supplier Material materials with Elastic modulus of 15 GPa

DIN EN ISO 527-1

Elongation

23.0 °C

1.8 %

Show Supplier Material materials with Elongation of 1.8 %

DIN EN ISO 527-1

Impact strength, Charpy unnotched

23.0 °C

32 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 32 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

200 MPa

Show Supplier Material materials with Tensile strength of 200 MPa

DIN EN ISO 527-1

Thermal

PropertyValue

Glass transition temperature

90 - 130 °C

Show Supplier Material materials with Glass transition temperature of 90 - 130 °C

Max service temperature, long

150 °C

Show Supplier Material materials with Max service temperature, long of 150 °C

Max service temperature, short

250 °C

Show Supplier Material materials with Max service temperature, short of 250 °C

Melting point

285 °C

Show Supplier Material materials with Melting point of 285 °C

Technological properties

Property
Application areas

Automotive industry: Seat (bumper, roll), Steering, Gear (shift handle and bearings), electronics (radar) and Mechanical engineering

Color

Black

Processing methods

Drying temperature (°C): 120, drying time (h): 5, mould temperature (°C): 120, material temperature (°C): , cylinder/processing temperature (°C): 315