TECACOMP PP ID blue 1061097

Alternative and trade names
PP-MD
Want to keep this datasheet? Save it now in your required format

Description

PP (Polypropylene) filled with detectable filler. Main features : detectable via metal detector , x-ray detectable, Explanation of food contact according to FDA and EU 10/2011 on request

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Elastic modulus of 2.3 GPa

DIN EN ISO 527-1

Elongation

23.0 °C

58 %

Show Supplier Material materials with Elongation of 58 %

DIN EN ISO 527-1

Impact strength, Charpy unnotched

23.0 °C

34 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 34 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

25 MPa

Show Supplier Material materials with Tensile strength of 25 MPa

DIN EN ISO 527-1

Thermal

PropertyValueComment

Glass transition temperature

13 °C

Show Supplier Material materials with Glass transition temperature of 13 °C

Max service temperature, long

100 °C

Show Supplier Material materials with Max service temperature, long of 100 °C

Max service temperature, short

130 °C

Show Supplier Material materials with Max service temperature, short of 130 °C

Melting point

165 °C

Show Supplier Material materials with Melting point of 165 °C

DIN 53765

Rheological Properties

PropertyValueComment

Melt mass-flow rate

4 g/10min

Show Supplier Material materials with Melt mass-flow rate of 4 g/10min

DIN EN ISO 1133, 230°C/2.16kg

Technological properties

Property
Certifications

Explanation of food contact according to FDA and EU 10/2011

Color

Blue

Fillers

Detectable Filler

Processing methods

Permissible residual moisture content (%): 0.1, drying temperature (°C): 70-100, drying time (h): 2, mould temperature (°C): 40-100, material temperature (°C): 230-250, cylinder/processing temperature (°C): 200-260