Description

PP (Polypropylen) for injection modling, with high electrical conductivity and thermal conductivity.

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.67 g/cm³

Show Supplier Material materials with Bulk density of 0.67 g/cm³

EN ISO 60

Density

23.0 °C

1.87 g/cm³

Show Supplier Material materials with Density of 1.87 g/cm³

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

max., DIN EN ISO 62, 23 °C / 50 % relative humidity up to saturation

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

16 GPa

Show Supplier Material materials with Elastic modulus of 16 GPa

DIN EN ISO 527-1

Flexural modulus

23.0 °C

7.2 GPa

Show Supplier Material materials with Flexural modulus of 7.2 GPa

DIN EN ISO 178

Flexural strain

23.0 °C

0.2 %

Show Supplier Material materials with Flexural strain of 0.2 %

DIN EN ISO 178

Flexural strength

23.0 °C

40 MPa

Show Supplier Material materials with Flexural strength of 40 MPa

DIN EN ISO 178

Impact strength, Charpy unnotched

23.0 °C

1.7 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 1.7 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

22 MPa

Show Supplier Material materials with Tensile strength of 22 MPa

DIN EN ISO 527-1

Thermal

PropertyTemperatureValueComment

Heat deflection temperature

148 °C

Show Supplier Material materials with Heat deflection temperature of 148 °C

Heat deflection temperature, 1.80 MPa

148 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 148 °C

ISO-R 75 Method A

Max service temperature

90 - 130 °C

Show Supplier Material materials with Max service temperature of 90 - 130 °C

Max service temperature, long

90 °C

Show Supplier Material materials with Max service temperature, long of 90 °C

Max service temperature, short

130 °C

Show Supplier Material materials with Max service temperature, short of 130 °C

Melting point

160 °C

Show Supplier Material materials with Melting point of 160 °C

DIN 53765

Specific heat capacity

23.0 °C

900 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 900 J/(kg·K)

DIN EN 821

Thermal conductivity

23.0 °C

24 - 45 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 24 - 45 W/(m·K)

Thermal conductivity, in-plane

23.0 °C

45 W/(m·K)

Show Supplier Material materials with Thermal conductivity, in-plane of 45 W/(m·K)

DIN EN 821

Thermal conductivity, through-plane

23.0 °C

24 W/(m·K)

Show Supplier Material materials with Thermal conductivity, through-plane of 24 W/(m·K)

DIN EN 821

Thermal diffusivity

23.0 °C

10.2 - 24 mm²/s

Show Supplier Material materials with Thermal diffusivity of 10.2 - 24 mm²/s

Thermal diffusivity, in-plane

23.0 °C

24 mm²/s

Show Supplier Material materials with Thermal diffusivity, in-plane of 24 mm²/s

DIN EN 821

Thermal diffusivity, through-plane

23.0 °C

10.2 mm²/s

Show Supplier Material materials with Thermal diffusivity, through-plane of 10.2 mm²/s

DIN EN 821

Flammability

UL94 class HB, DIN IEC 60695-11-10

Electrical

PropertyTemperatureValueComment

Electrical conductivity

23.0 °C

2500 S/m

Show Supplier Material materials with Electrical conductivity of 2500 S/m

DIN EN ISO 3915

Volume resistivity

23.0 °C

3.9E-3 Ω·cm

Show Supplier Material materials with Volume resistivity of 3.9E-3 Ω·cm

DIN EN 61340-2-3

Technological properties

Property
Application areas

Bipolar plates for PEM fuel cells, heat exchanger and Separator plates for Redox Flow Batteries

Color

Black

Fillers

Graphite