General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.05 g/cm³ Show Supplier Material materials with Density of 1.05 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 2.15 GPa Show Supplier Material materials with Elastic modulus of 2.15 GPa at 23.0 °C | 23.0 °C | ASTM D638 |
Elongation | 30 % Show Supplier Material materials with Elongation of 30 % at 23.0 °C | 23.0 °C | ASTM D638 |
Flexural modulus | 2.35 GPa Show Supplier Material materials with Flexural modulus of 2.35 GPa at 23.0 °C | 23.0 °C | ASTM D790 |
Flexural strength | 67.35 MPa Show Supplier Material materials with Flexural strength of 67.35 MPa at 23.0 °C | 23.0 °C | ASTM D790 |
Impact strength, Izod notched, ASTM | 250 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250 J/m at 23.0 °C | 23.0 °C | ASTM D256 |
Tensile strength | 42.5 MPa Show Supplier Material materials with Tensile strength of 42.5 MPa at 23.0 °C | 23.0 °C | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Flammability | UL-94 1/16‘ HB | |
Melting point | 180 - 200 °C Show Supplier Material materials with Melting point of 180 - 200 °C | ISO 3146-C |
Vicat softening temperature | 94 °C Show Supplier Material materials with Vicat softening temperature of 94 °C | ASTM D1525 |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 44 g/10min Show Supplier Material materials with Melt mass-flow rate of 44 g/10min | ASTM D1238 | |
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % at 23.0 °C | 23.0 °C | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | The strength, flexibility, machinability and high-temperature resistance of ABS often makes it the plastic preferred by engineers and people intending to use plastic in a mechanical context. | |
Certifications | Extrudr ABS can be used in applications for direct/indirect food contact under the FDA regulation | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |