General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.22 g/cm³ Show Supplier Material materials with Density of 1.22 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Flexural modulus | 3.5 GPa Show Supplier Material materials with Flexural modulus of 3.5 GPa at 23.0 °C | 23.0 °C | ASTM D882 |
Impact strength, Izod notched, ASTM | 16 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 16 J/m at 23.0 °C | 23.0 °C | ASTM D256 |
Tensile strength | 61 MPa Show Supplier Material materials with Tensile strength of 61 MPa at 23.0 °C | 23.0 °C | ASTM D882 |
Thermal
Property | Value | Comment |
---|---|---|
Melting point | 190 - 200 °C Show Supplier Material materials with Melting point of 190 - 200 °C | ISO 3146-C |
Vicat softening temperature | 60 °C Show Supplier Material materials with Vicat softening temperature of 60 °C | ISO 306 |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 6.5 g/10min Show Supplier Material materials with Melt mass-flow rate of 6.5 g/10min | ASTM D1238 | |
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % at 23.0 °C | 23.0 °C | ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Application areas | PLA is used to make an increasingly wide variety of products. PLA can be used in rapid prototyping, architecture, food applications, toys and outdoor novelties. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |