extrudr PETG Filament

Alternative and trade names
extrudr PETG Filament
Want to keep this datasheet? Save it now in your required format

Description

Polyethylene Terephthalate Glycol (PETG) is one of the world‘s most common thermoplastic polymers.

This material data has been provided by extrudr.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elastic modulus

2.04 GPa

Show Supplier Material materials with Elastic modulus of 2.04 GPa

ISO 178

Elongation

29.0 %

Show Supplier Material materials with Elongation of 29.0 %

ISO 527

Flexural modulus

3.1 GPa

Show Supplier Material materials with Flexural modulus of 3.1 GPa

ISO 527

Flexural strength

68.3 MPa

Show Supplier Material materials with Flexural strength of 68.3 MPa

ISO 178

Tensile strength

50.0 MPa

Show Supplier Material materials with Tensile strength of 50.0 MPa

ISO 527

Thermal

PropertyValueComment

Melting point

180.0 - 200.0 °C

Show Supplier Material materials with Melting point of 180.0 - 200.0 °C

ISO 3146-C

Vicat softening temperature

78 °C

Show Supplier Material materials with Vicat softening temperature of 78 °C

ISO 306

Rheological Properties

PropertyValueComment

Melt mass-flow rate

7.0 g/10min

Show Supplier Material materials with Melt mass-flow rate of 7.0 g/10min

ISO 1133

Shrinkage

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

ISO 294-4

Technological properties

Property
Application areas

PETG is specifically designed to have a large and general scope of application in situations where the main requirement is the balance between mechanical and optical material properties.

Handling recommendations

Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year.