General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.05 g/cm³ Show Supplier Material materials with Density of 1.05 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 2.06 GPa Show Supplier Material materials with Elastic modulus of 2.06 GPa at 23.0 °C | 23.0 °C | ASTM D638 |
Elongation | 26 % Show Supplier Material materials with Elongation of 26 % at 23.0 °C | 23.0 °C | ASTM D638 |
Flexural modulus | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa at 23.0 °C | 23.0 °C | ASTM D790 |
Flexural strength | 74.5 MPa Show Supplier Material materials with Flexural strength of 74.5 MPa at 23.0 °C | 23.0 °C | ASTM D790 |
Impact strength, Izod notched, ASTM | 167 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 167 J/m at 23.0 °C | 23.0 °C | ASTM D256 |
Tensile strength | 47.6 MPa Show Supplier Material materials with Tensile strength of 47.6 MPa at 23.0 °C | 23.0 °C | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Flammability | UL-94 HB | |
Melting point | 180 - 200 °C Show Supplier Material materials with Melting point of 180 - 200 °C | ISO 3146-C |
Vicat softening temperature | 98 °C Show Supplier Material materials with Vicat softening temperature of 98 °C | ASTM D1525 |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 12 g/10min Show Supplier Material materials with Melt mass-flow rate of 12 g/10min | ASTM D1238 | |
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % at 23.0 °C | 23.0 °C | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | The strength, machinibility, durability and weatherability makes ASA the prefered replacement for ABS. It has a higher impact resistance and is ideal for outdoor use due to its UV resistance. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |