General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ at 23.0 °C | 23.0 °C | ISO 2781 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Hardness, Shore D | 58 [-] Show Supplier Material materials with Hardness, Shore D of 58 [-] at 23.0 °C | 23.0 °C | ISO 868 |
Tear Strength Unnicked | 171 kN/m Show Supplier Material materials with Tear Strength Unnicked of 171 kN/m at 23.0 °C | 23.0 °C | ISO 34-1B |
Tensile strength | 42 MPa Show Supplier Material materials with Tensile strength of 42 MPa at 23.0 °C | 23.0 °C | ISO 527-2 |
Thermal
Property | Value | Comment |
---|---|---|
Melting point | 180 - 200 °C Show Supplier Material materials with Melting point of 180 - 200 °C | ISO 3146-C |
Vicat softening temperature | 137 °C Show Supplier Material materials with Vicat softening temperature of 137 °C | ISO 306 |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its chemical and mechanical resistance, TPU is primarily used in the car and footwear industry. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |