extrudr Flex Medium Filament (TPU)

Alternative and trade names
extrudr Flex Medium Filament
Want to keep this datasheet? Save it now in your required format

Description

The Extrudr TPU Flex line, which features Extrudr TPU Flex in varying degrees of hardness, has been developed mainly for use with industrial machinery.

This material data has been provided by extrudr.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.15 g/cm³

Show Supplier Material materials with Density of 1.15 g/cm³

ISO 2781

Mechanical

PropertyValueComment

Hardness, Shore A

98.0 [-]

Show Supplier Material materials with Hardness, Shore A of 98.0 [-]

ISO 868

Tear Strength Unnicked

176.0 kN/m

Show Supplier Material materials with Tear Strength Unnicked of 176.0 kN/m

ISO 34-1B

Tensile strength

42.0 MPa

Show Supplier Material materials with Tensile strength of 42.0 MPa

ISO 527-2

Thermal

PropertyValueComment

Melting point

180.0 - 200.0 °C

Show Supplier Material materials with Melting point of 180.0 - 200.0 °C

ISO 3146-C

Vicat softening temperature

110 °C

Show Supplier Material materials with Vicat softening temperature of 110 °C

ISO 306

Technological properties

Property
Application areas

Due to its chemical and mechanical resistance, TPU is primarily used in the car and footwear industry.

Handling recommendations

Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year.