extrudr GreenTEC Filament

Alternative and trade names
extrudr GreenTEC Filament
Want to keep this datasheet? Save it now in your required format

Description

GreenTEC is made from a high-performance renewable biodegradable biopolymer.

This material data has been provided by extrudr.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bio-based content

100 %

Show Supplier Material materials with Bio-based content of 100 %

Density

23.0 °C

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

14 %

Show Supplier Material materials with Elongation of 14 %

ISO 527

Flexural modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Flexural modulus of 3.3 GPa

ISO 527

Impact strength, Charpy notched

23.0 °C

19 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 19 kJ/m²

ISO 179-1/1 eA

Impact strength, Charpy unnotched

23.0 °C

218 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 218 kJ/m²

ISO 179-1/1 eU

Tensile strength

23.0 °C

45 MPa

Show Supplier Material materials with Tensile strength of 45 MPa

ISO 527

Thermal

PropertyValueComment

Heat deflection temperature

47 °C

Show Supplier Material materials with Heat deflection temperature of 47 °C

Heat deflection temperature, 0.45 MPa

47 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 47 °C

ISO 75/B

Melting point

180 - 200 °C

Show Supplier Material materials with Melting point of 180 - 200 °C

ISO 3146-C

Vicat softening temperature

115 °C

Show Supplier Material materials with Vicat softening temperature of 115 °C

ISO 306

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

3.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 3.5 g/10min

ISO 1133

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

ISO 294-4

Technological properties

Property
Application areas

GreenTEC is designed for industrial use. It has good mechanical and thermal properties.

Handling recommendations

Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year.