extrudr GreenTEC PRO Filament

Alternative and trade names
extrudr GreenTEC PRO Filament
Want to keep this datasheet? Save it now in your required format

Description

GreenTEC PRO is made from a high-performance and heat-resistant renewable biodegradable biopolymer.

This material data has been provided by extrudr.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

ISO 527

Flexural modulus

23.0 °C

4.4 GPa

Show Supplier Material materials with Flexural modulus of 4.4 GPa

ISO 527

Impact strength, Charpy notched

23.0 °C

4.4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 4.4 kJ/m²

ISO 179-1/1 eA

Impact strength, Charpy unnotched

23.0 °C

72 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 72 kJ/m²

ISO 179-1/1 eU

Tensile strength

23.0 °C

61 MPa

Show Supplier Material materials with Tensile strength of 61 MPa

ISO 527

Thermal

PropertyValueComment

Melting point

190 - 210 °C

Show Supplier Material materials with Melting point of 190 - 210 °C

ISO 3146-C

Vicat softening temperature

160 °C

Show Supplier Material materials with Vicat softening temperature of 160 °C

ISO 306

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

12 g/10min

Show Supplier Material materials with Melt mass-flow rate of 12 g/10min

ISO 1133

Shrinkage

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

ISO 294-4

Technological properties

Property
Application areas

GreenTEC PRO is designed for extreme industrial use. It has very good mechanical and thermal properties.

Handling recommendations

Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year.