General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 19.3 g/cm³ Show Supplier Material materials with Density of 19.3 g/cm³ |
Molar mass | 183.85 g/mol Show Supplier Material materials with Molar mass of 183.85 g/mol | |
Neutron capture cross-section | 23.0 °C | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 405 GPa Show Supplier Material materials with Elastic modulus of 405 GPa | |
Hardness, Vickers, 30 | 23.0 °C | 360 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 360 [-] | recrystallized |
Poisson's ratio | 23.0 °C | 0.28 [-] Show Supplier Material materials with Poisson's ratio of 0.28 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Melting point | 3420 °C Show Supplier Material materials with Melting point of 3420 °C | |
Specific heat capacity | 23.0 °C | 130 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 130 J/(kg·K) |
Thermal conductivity | 23.0 °C | 164 W/(m·K) Show Supplier Material materials with Thermal conductivity of 164 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.80E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.80E+7 S/m |
Electrical resistivity | 23.0 °C | 5E-8 Ω·m Show Supplier Material materials with Electrical resistivity of 5E-8 Ω·m |
Electron work function | 23.0 °C | 4.54 eV Show Supplier Material materials with Electron work function of 4.54 eV |
Acoustical
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Carbon | 6E-4 % Show Supplier Material materials with Carbon of 6E-4 % |
Chromium | 3E-4 % Show Supplier Material materials with Chromium of 3E-4 % |
Copper | 1E-4 % Show Supplier Material materials with Copper of 1E-4 % |
Iron | 8E-4 % Show Supplier Material materials with Iron of 8E-4 % |
Lead | 1E-4 % Show Supplier Material materials with Lead of 1E-4 % |
Molybdenum | 1.2E-3 % Show Supplier Material materials with Molybdenum of 1.2E-3 % |
Nickel | 2E-4 % Show Supplier Material materials with Nickel of 2E-4 % |
Nitrogen | 1E-4 % Show Supplier Material materials with Nitrogen of 1E-4 % |
Oxygen | 2E-4 % Show Supplier Material materials with Oxygen of 2E-4 % |
Potassium | 1E-4 % Show Supplier Material materials with Potassium of 1E-4 % |
Silicon | 1E-4 % Show Supplier Material materials with Silicon of 1E-4 % |
Tungsten | 99.97 % Show Supplier Material materials with Tungsten of 99.97 % |
Technological properties
Property | ||
---|---|---|
Application areas | For example, this material can be used to manufacture high-temperature furnace components, lamp components and components for use in the fields of medical and thin-film technology. |