PropertyTemperatureValue

Density

23.0 °C

17.55 g/cm³

Show Supplier Material materials with Density of 17.55 g/cm³

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

11 %

Show Supplier Material materials with Elongation of 11 %

Impact strength, Charpy notched

23.0 °C

1500 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 1500 kJ/m²

(5x5)

Tensile strength

23.0 °C

1435 MPa

Show Supplier Material materials with Tensile strength of 1435 MPa

Yield strength

23.0 °C

1410 MPa