Density ρ
17.6 g/cm³ at 20 °C
Elongation A
11 % at 20 °C
Impact strength, Charpy notched Ivnot
1500 kJ/m² at 20 °C
(5x5)
Tensile strength Rm
1460 MPa at 20 °C
Yield strength YS
1460 MPa at 20 °C
This material data has been provided by Plansee.