Plansee Densimet® composite materials are heavy metals with a high tungsten content (> 90%) and a NiFe binder phase.
Diameter d
6 mm
Length l
330 mm
Density ρ
17.15 - 17.85 g/cm³ at 20 °C
Dimension
Available dimensions (diameter x length, mm x mm): 6 x 330; 8 x 330; 10 x 330; 12 x 330; 14 x 320; 16 x 320; 18 x 320; 20 x 500; 22 x 500; 24 x 500; 26 x 500; 28 x 500; 30 x 500; 32 x 500; 37 x 500; 42 x 600; 47 x 600; 52 x 600; 57 x 700; 62 x 700
Elastic modulus E
360 GPa at 20 °C
Hardness, Vickers, 10 HV 10
270 - 330 [-] at 20 °C
Yield strength Rp0.2 Rp0.2
517 MPa at 20 °C
Element
Weight %
Comment
91.5 - 93.5 %
4.5 - 5.5 %
2 - 3 %
Application areas
Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry.
Other
Weakly ferromagnetic, DENSIMET® D176 is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006.