Densimet® D2M Tungsten Heavy Alloy Turned Rod

Want to keep this datasheet? Save it now in your required format

Description

Plansee Densimet® composite materials are heavy metals with a high tungsten content (> 90%) and a NiFe binder phase.

Related Standards

Equivalent Materials

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

16.9 - 17.6 g/cm³

Show Supplier Material materials with Density of 16.9 - 17.6 g/cm³

Dimension

PropertyValue

Diameter

10 - 40 mm

Show Supplier Material materials with Diameter of 10 - 40 mm

Length

250 - 500 mm

Show Supplier Material materials with Length of 250 - 500 mm

Dimensions

Available dimensions (diameter x length, mm x mm): 10 x 250; 12 x 250; 16 x 250; 20 x 500; 25 x 500; 30 x 500; 40 x 500

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

360 GPa

Show Supplier Material materials with Elastic modulus of 360 GPa

Elongation

23.0 °C

4 - 18 %

Show Supplier Material materials with Elongation of 4 - 18 %

Hardness, Rockwell C

23.0 °C

31 [-]

Show Supplier Material materials with Hardness, Rockwell C of 31 [-]

Hardness, Vickers, 10

23.0 °C

300 - 360 [-]

Show Supplier Material materials with Hardness, Vickers, 10 of 300 - 360 [-]

Tensile strength

23.0 °C

800 - 990 MPa

Show Supplier Material materials with Tensile strength of 800 - 990 MPa

Yield strength

23.0 °C

700 MPa

Show Supplier Material materials with Yield strength of 700 MPa

Yield strength Rp0.2

23.0 °C

550 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 550 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

5.3E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.3E-6 1/K

Thermal conductivity

500.0 °C

65 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 65 W/(m·K)

Chemical properties

PropertyValue

Iron

1.5 - 2.5 %

Show Supplier Material materials with Iron of 1.5 - 2.5 %

Molybdenum

3.5 - 4.5 %

Show Supplier Material materials with Molybdenum of 3.5 - 4.5 %

Nickel

3.5 - 4.5 %

Show Supplier Material materials with Nickel of 3.5 - 4.5 %

Tungsten

88.5 - 91.5 %

Show Supplier Material materials with Tungsten of 88.5 - 91.5 %

Technological properties

Property
Application areas

Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry.

Other

Weakly ferromagnetic, DENSIMET® D2M is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006.