This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Plansee Inermet® composite materials are heavy metals with a high tungsten content (> 90%) and a NiCu binder phase.
Density ρ
17.6 g/cm³ at 20 °C
Elastic modulus E
350 GPa at 20 °C
Element
Weight %
Comment
-
binder
-
binder
92.5 %
Application areas
Inermet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry.
Other
Paramagnetic
This material data has been provided by Plansee.