This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.

The material: 'Molybdenum Deep Drawable Sheet 1 mm' you were looking for has been superseded by the one below.

Molybdenum Deep Drawable Sheet

.XLSX
.PDF
Save

Description

With its unique mechanical and chemical properties, molybdenum is an outstanding material that can meet the most exacting requirements. Because molybdenum possesses a very high melting point, a low coefficient of thermal expansion and a high level of thermal conductivity, it is used in many different industries. Molybdenum is a genuine all-rounder.

Related Standards

Properties

Acoustical

Sound speed, longitudinal clong

6250 m/s at 20 °C

Sound speed, transversal ctrans

3350 m/s at 20 °C

Dimension

Length l

2000 mm

Thickness t

0.15 - 1 mm

Width w

600 mm

Electrical

Electron work function We

4.39 eV at 20 °C

General

Density ρ

10.2 g/cm³ at 20 °C

Neutron capture cross-section σN

0 m² at 20 °C

Surface roughness RMS

0.2 μm

Material Information

Dimension

Available dimensions (width x length x thickness, mm x mm x mm): 600 x 2000 x 0.15; 600 x 2000 x 0.2; 600 x 2000 x 0.25; 600 x 2000 x 0.3; 600 x 2000 x 0.4; 600 x 2000 x 0.5; 600 x 2000 x 1

Mechanical

Elongation A

2 - 10 % at 20 °C

Hardness, Vickers HV

240 - 280 [-] at 20 °C

Tensile strength Rm

680 - 700 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

590 - 620 MPa at 20 °C

Thermal

Melting point Tm

2620 °C

Chemical properties

Element

Weight %

Comment

Mo

99.97 %

W

0.02 %

C

1.3000000000000002E-3 %

O

6.000000000000001E-4 %

K

6.000000000000001E-4 %

More

Technological properties

Application areas

Premium Quality sheets are used for many applications where superior finish is desired. It is ideal for deep drawing.

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.