General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Density of 10.2 g/cm³ |
Neutron capture cross-section | 23.0 °C | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² |
Surface roughness | 0.2 μm Show Supplier Material materials with Surface roughness of 0.2 μm |
Dimension
Property | Value |
---|---|
Length | 2000 mm Show Supplier Material materials with Length of 2000 mm |
Thickness | 0.15 - 1 mm Show Supplier Material materials with Thickness of 0.15 - 1 mm |
Width | 600 mm Show Supplier Material materials with Width of 600 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 600 x 2000 x 0.15; 600 x 2000 x 0.2; 600 x 2000 x 0.25; 600 x 2000 x 0.3; 600 x 2000 x 0.4; 600 x 2000 x 0.5; 600 x 2000 x 1 |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 2 - 10 % Show Supplier Material materials with Elongation of 2 - 10 % |
Hardness, Vickers | 23.0 °C | 240 - 280 [-] Show Supplier Material materials with Hardness, Vickers of 240 - 280 [-] |
Tensile strength | 23.0 °C | 680 - 700 MPa Show Supplier Material materials with Tensile strength of 680 - 700 MPa |
Yield strength Rp0.2 | 23.0 °C | 590 - 620 MPa Show Supplier Material materials with Yield strength Rp0.2 of 590 - 620 MPa |
Thermal
Property | Value |
---|---|
Melting point | 2620 °C Show Supplier Material materials with Melting point of 2620 °C |
Electrical
Property | Temperature | Value |
---|---|---|
Electron work function | 23.0 °C | 4.39 eV Show Supplier Material materials with Electron work function of 4.39 eV |
Acoustical
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Carbon | 1.3E-3 % Show Supplier Material materials with Carbon of 1.3E-3 % |
Chromium | 3E-4 % Show Supplier Material materials with Chromium of 3E-4 % |
Copper | 2E-4 % Show Supplier Material materials with Copper of 2E-4 % |
Iron | 5E-4 % Show Supplier Material materials with Iron of 5E-4 % |
Molybdenum | 99.97 % Show Supplier Material materials with Molybdenum of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Nitrogen | 5E-4 % Show Supplier Material materials with Nitrogen of 5E-4 % |
Oxygen | 6E-4 % Show Supplier Material materials with Oxygen of 6E-4 % |
Potassium | 6E-4 % Show Supplier Material materials with Potassium of 6E-4 % |
Silicon | 2E-4 % Show Supplier Material materials with Silicon of 2E-4 % |
Tungsten | 0.02 % Show Supplier Material materials with Tungsten of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Premium Quality sheets are used for many applications where superior finish is desired. It is ideal for deep drawing. |