Molybdenum Tantalum Alloy (MT11)

Alternative and trade names
MoTa
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Grain structure

Fine-grained, homogeneous

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

5.34E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.34E-6 1/K at 23.0 °C

23.0 °C

Thermal conductivity

97 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 97 W/(m·K) at 23.0 °C

23.0 °C

Electrical

PropertyValueTemperature

Electrical conductivity

1.30E+7 S/m

Show Supplier Material materials with Electrical conductivity of 1.30E+7 S/m at 23.0 °C

23.0 °C

Chemical properties

Property

Molybdenum

balance

Tantalum

10.75 %

Technological properties

Property
Application areas

Thanks to its good adherence to glass and a high level of electrical conductivity, molybdenum is a popular material for electrode layers in thin-film transistors (TFT-LCD) and touch sensors (touch panels).