Description

MY is a particle-reinforced molybdenum alloy that contains 0.47 percent yttrium oxide by weight and 0.08 percent cerium oxide by weight. MY adheres well to quartz glass, is easy to weld and provides better resistance to oxidation than pure molybdenum.

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

10.1 g/cm³

Show Supplier Material materials with Density of 10.1 g/cm³

Surface roughness

0.15 μm

Show Supplier Material materials with Surface roughness of 0.15 μm

Dimension

PropertyValue

Thickness

0.02 - 0.04 mm

Show Supplier Material materials with Thickness of 0.02 - 0.04 mm

Width

1.5 - 10 mm

Show Supplier Material materials with Width of 1.5 - 10 mm

Dimensions

Available dimensions (width x thickness, mm x mm): 1.5 x 0.02; 2 x 0.025; 3 x 0.025; 4 x 0.025; 2 x 0.028; 2.5 x 0.028; 3 x 0.028; 4 x 0.028; 3 x 0.03; 4.8 x 0.033; 5 x 0.035; 6 x 0.035; 10 x 0.04

Mechanical

PropertyTemperatureValue

Tensile strength

23.0 °C

750 - 1000 MPa

Show Supplier Material materials with Tensile strength of 750 - 1000 MPa

Chemical properties

PropertyValueComment

Aluminium

1E-4 %

Show Supplier Material materials with Aluminium of 1E-4 %

Cadmium

1E-4 %

Show Supplier Material materials with Cadmium of 1E-4 %

Carbon

1.3E-3 %

Show Supplier Material materials with Carbon of 1.3E-3 %

Cerium

0.08 %

Show Supplier Material materials with Cerium of 0.08 %

as CeO₂

Chromium

3E-4 %

Show Supplier Material materials with Chromium of 3E-4 %

Copper

2E-4 %

Show Supplier Material materials with Copper of 2E-4 %

Iron

5E-4 %

Show Supplier Material materials with Iron of 5E-4 %

Molybdenum

balance

Nickel

1E-4 %

Show Supplier Material materials with Nickel of 1E-4 %

Nitrogen

1E-4 %

Show Supplier Material materials with Nitrogen of 1E-4 %

Potassium

4E-4 %

Show Supplier Material materials with Potassium of 4E-4 %

Silicon

2E-4 %

Show Supplier Material materials with Silicon of 2E-4 %

Tungsten

0.02 %

Show Supplier Material materials with Tungsten of 0.02 %

Yttrium

0.47 - 0.6 %

Show Supplier Material materials with Yttrium of 0.47 - 0.6 %

as Y-mixed oxide

Technological properties

Property
Application areas

MY is primarily used in conductive ESS ribbons and in evaporation boats for applications in the field of coating technology and in the lighting industry.

Other