Molybdenum Yttrium Cerium Oxide (MY) Pickled Strip

.XLSX
.PDF
Save

Description

MY is a particle-reinforced molybdenum alloy that contains 0.47 percent yttrium oxide by weight and 0.08 percent cerium oxide by weight. MY adheres well to quartz glass, is easy to weld and provides better resistance to oxidation than pure molybdenum.

Properties

Dimension

Thickness t

0.02 - 0.04 mm

Width w

1.5 - 10 mm

General

Density ρ

10.1 g/cm³ at 20 °C

Surface roughness RMS

0.15 μm

Material Information

Dimension

Available dimensions (width x thickness, mm x mm): 1.5 x 0.02; 2 x 0.025; 3 x 0.025; 4 x 0.025; 2 x 0.028; 2.5 x 0.028; 3 x 0.028; 4 x 0.028; 3 x 0.03; 4.8 x 0.033; 5 x 0.035; 6 x 0.035; 10 x 0.04

Mechanical

Tensile strength Rm

750 - 1000 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mo

-

balance

Y

0.47 - 0.6 %

as Y-mixed oxide

Ce

0.08 %

as CeO₂

W

0.02 %

C

1.3000000000000002E-3 %

More

Technological properties

Application areas

MY is primarily used in conductive ESS ribbons and in evaporation boats for applications in the field of coating technology and in the lighting industry.

Other

ESS (Elliptically Shaped for Sealing-in) Ribbon with tapered edges by etching.

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.