General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Density of 10.1 g/cm³ |
Surface roughness | 0.15 μm Show Supplier Material materials with Surface roughness of 0.15 μm |
Dimension
Property | Value |
---|---|
Thickness | 0.02 - 0.04 mm Show Supplier Material materials with Thickness of 0.02 - 0.04 mm |
Width | 1.5 - 10 mm Show Supplier Material materials with Width of 1.5 - 10 mm |
Dimensions | Available dimensions (width x thickness, mm x mm): 1.5 x 0.02; 2 x 0.025; 3 x 0.025; 4 x 0.025; 2 x 0.028; 2.5 x 0.028; 3 x 0.028; 4 x 0.028; 3 x 0.03; 4.8 x 0.033; 5 x 0.035; 6 x 0.035; 10 x 0.04 |
Mechanical
Property | Temperature | Value |
---|---|---|
Tensile strength | 23.0 °C | 750 - 1000 MPa Show Supplier Material materials with Tensile strength of 750 - 1000 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % | ||
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | ||
Carbon | 1.3E-3 % Show Supplier Material materials with Carbon of 1.3E-3 % | ||
Cerium | 0.08 % Show Supplier Material materials with Cerium of 0.08 % | as CeO₂ | |
Chromium | 3E-4 % Show Supplier Material materials with Chromium of 3E-4 % | ||
Copper | 2E-4 % Show Supplier Material materials with Copper of 2E-4 % | ||
Iron | 5E-4 % Show Supplier Material materials with Iron of 5E-4 % | ||
Molybdenum | balance | ||
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % | ||
Nitrogen | 1E-4 % Show Supplier Material materials with Nitrogen of 1E-4 % | ||
Potassium | 4E-4 % Show Supplier Material materials with Potassium of 4E-4 % | ||
Silicon | 2E-4 % Show Supplier Material materials with Silicon of 2E-4 % | ||
Tungsten | 0.02 % Show Supplier Material materials with Tungsten of 0.02 % | ||
Yttrium | 0.47 - 0.6 % Show Supplier Material materials with Yttrium of 0.47 - 0.6 % | as Y-mixed oxide |
Technological properties
Property | ||
---|---|---|
Application areas | MY is primarily used in conductive ESS ribbons and in evaporation boats for applications in the field of coating technology and in the lighting industry. | |
Other | ESS (Elliptically Shaped for Sealing-in) Ribbon with tapered edges by etching. |