Molybdenum Rhenium Alloy (MoRe5)

Want to keep this datasheet? Save it now in your required format

Description

Small quantities of rhenium make molybdenum ductile even below room temperature.

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Molybdenum

balance

Rhenium

5 %

Show Supplier Material materials with Rhenium of 5 %

Technological properties

Property
Application areas

Molybdenum-rhenium (MoRe) is primarily used for thermocouple wires in the standard compositions MoRe5 and MoRe41 as well as in applications where a high level of ductility is important.