Description

Tungsten has the highest melting point of all metals and is therefore also suitable for very high-temperature applications. It is also characterized by a uniquely low coefficient of thermal expansion and a very high level of dimensional stability.

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

19.1 g/cm³

Show Supplier Material materials with Density of 19.1 g/cm³

Neutron capture cross-section

23.0 °C

0 m²

Show Supplier Material materials with Neutron capture cross-section of 0 m²

Surface roughness

1 μm

Show Supplier Material materials with Surface roughness of 1 μm

Dimension

PropertyValue

Diameter

2 - 25.4 mm

Show Supplier Material materials with Diameter of 2 - 25.4 mm

Length

300 - 2900 mm

Show Supplier Material materials with Length of 300 - 2900 mm

Dimensions

Available dimensions (diameter x length, mm x mm): 2 x 500-2900; 2.54 x 500-2900; 3 x 500-2900; 3.175 x 500-2900; 4 x 500-2300; 4.75 x 500-2400; 5 x 500-2400; 6 x 500-2400; 6.35 x 500-2400; 8 x 500-2000; 10 x 500-2700; 12 x 300-1800; 12.7 x 300-1600; 14 x 300-1300; 16 x 300-1600; 18 x 300-2200; 19.05 x 300-1800; 20 x 300-1700; 25 x 300-2400; 25.4 x 300-2300

Thermal

PropertyValue

Melting point

3420 °C

Show Supplier Material materials with Melting point of 3420 °C

Electrical

PropertyTemperatureValue

Electron work function

23.0 °C

4.54 eV

Show Supplier Material materials with Electron work function of 4.54 eV

Acoustical

PropertyTemperatureValue

Sound speed, longitudinal

23.0 °C

5180 m/s

Show Supplier Material materials with Sound speed, longitudinal of 5180 m/s

Sound speed, transversal

23.0 °C

2870 m/s

Show Supplier Material materials with Sound speed, transversal of 2870 m/s

Chemical properties

PropertyValue

Aluminium

1E-4 %

Show Supplier Material materials with Aluminium of 1E-4 %

Cadmium

1E-4 %

Show Supplier Material materials with Cadmium of 1E-4 %

Carbon

6E-4 %

Show Supplier Material materials with Carbon of 6E-4 %

Chromium

3E-4 %

Show Supplier Material materials with Chromium of 3E-4 %

Copper

1E-4 %

Show Supplier Material materials with Copper of 1E-4 %

Iron

8E-4 %

Show Supplier Material materials with Iron of 8E-4 %

Lead

1E-4 %

Show Supplier Material materials with Lead of 1E-4 %

Molybdenum

1.2E-3 %

Show Supplier Material materials with Molybdenum of 1.2E-3 %

Nickel

2E-4 %

Show Supplier Material materials with Nickel of 2E-4 %

Nitrogen

1E-4 %

Show Supplier Material materials with Nitrogen of 1E-4 %

Oxygen

2E-4 %

Show Supplier Material materials with Oxygen of 2E-4 %

Potassium

1E-4 %

Show Supplier Material materials with Potassium of 1E-4 %

Silicon

1E-4 %

Show Supplier Material materials with Silicon of 1E-4 %

Tungsten

99.97 %

Show Supplier Material materials with Tungsten of 99.97 %

Technological properties

Property
Application areas