RADILON DT RV500RKC2 306 BK

Alternative and trade names
PA612-T GF50, PA612-GF50
Want to keep this datasheet? Save it now in your required format

Description

PA612, 50% glass fibre reinforced injection moulding grade. Heat stabilized, improved flowability. Black colour

Suitable for parts requiring very high stiffness and high mechanical resistance in direct contact with drinking water and food. Excellent dimensional stability, improved hydrolytic stability and chemical resistance to disinfectants up to 60°C. Product developed for applications in civil and industrial water management as well as appliances.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.51 g/cm³

Show Supplier Material materials with Density of 1.51 g/cm³

ISO 1183, DAM

Moisture absorption

23.0 °C

0.6 %

Show Supplier Material materials with Moisture absorption of 0.6 %

ISO 62, 50% RH, thickness tested (mm): 2

Water absorption

23.0 °C

1.5 %

Show Supplier Material materials with Water absorption of 1.5 %

ISO 62, thickness tested (mm): 2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

14.9 GPa

Show Supplier Material materials with Elastic modulus of 14.9 GPa

ISO 527-2/1A, 1mm/min, DAM

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

ISO 527-2/1A, 5mm/min, DAM

Flexural modulus

23.0 °C

13 GPa

Show Supplier Material materials with Flexural modulus of 13 GPa

ISO 178, 2mm/min, DAM

Flexural strength

23.0 °C

295 MPa

Show Supplier Material materials with Flexural strength of 295 MPa

ISO 178, 2mm/min, DAM

Impact strength, Charpy notched

23.0 °C

14 - 30 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 14 - 30 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-30.0 °C

80 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m²

ISO 179/1eU

23.0 °C

95 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m²

ISO 179/1eU

Tensile strength

23.0 °C

190 MPa

Show Supplier Material materials with Tensile strength of 190 MPa

ISO 527-2/1A, 5mm/min, DAM

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C

ISO 75/2Af

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ISO 11357-1/-3, 10°C/min

Flammability

Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 | Class: HB ,method: UL 94, and thickness tested (mm): 1.6

Electrical

PropertyTemperatureValueComment

Volume resistivity

23.0 °C

1.00E+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm

IEC 60093, 500V, DAM

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

ISO 294-4, DAM

Shrinkage, transverse

23.0 °C

0.6 %

Show Supplier Material materials with Shrinkage, transverse of 0.6 %

ISO 294-4, DAM

Technological properties

Property
Certifications

RoHS 2011/65/UE, Food and Water Contact (please get in touch with Radici Group): KTW guidlines and DVGW-standard W270 (11/2007), ACS (certificate of sanitary conformity)

Color

Black

Fillers

50% Glass Fiber

Processing methods

Injection Molding