RADISTRONG AROMA RV500RKC2 306 BK

Alternative and trade names
PA66-GF50
Want to keep this datasheet? Save it now in your required format

Description

Special PA 50% glass fibre reinforced, high flow injection moulding grade. Heat stabilized. Drinking water and food contact. Black colour.

Product with high mechanical properties intended for use in direct contact with drinking water and food, along with good hydrolytic stability and chemical resistance to disinfectants. This grade has also high surface quality and high gloss. Suitable for applications in civil and industrial water management as well as appliances.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.59 g/cm³

Show Supplier Material materials with Density of 1.59 g/cm³

ISO 1183, DAM

Moisture absorption

23.0 °C

1.2 %

Show Supplier Material materials with Moisture absorption of 1.2 %

ISO 62, 50% RH, thickness tested (mm): 2

Water absorption

ISO 62, thickness tested (mm): 2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

17.9 GPa

Show Supplier Material materials with Elastic modulus of 17.9 GPa

ISO 527-2/1A, 1mm/min, DAM

Elongation

23.0 °C

2.4 %

Show Supplier Material materials with Elongation of 2.4 %

ISO 527-2/1A, 5mm/min, DAM

Flexural modulus

23.0 °C

15.2 GPa

Show Supplier Material materials with Flexural modulus of 15.2 GPa

ISO 178, 2mm/min, DAM

Flexural strength

23.0 °C

355 MPa

Show Supplier Material materials with Flexural strength of 355 MPa

ISO 178, 2mm/min, DAM

Impact strength, Charpy notched

23.0 °C

-30 - 15.5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of -30 - 15.5 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

98 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 98 kJ/m²

ISO 179/1eU

Tensile strength

23.0 °C

240 MPa

Show Supplier Material materials with Tensile strength of 240 MPa

ISO 527-2/1A, 5mm/min, DAM

Thermal

PropertyValueComment

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 11357-1/-3, 10°C/min

Flammability

Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

ISO 294-4, DAM

Shrinkage, transverse

23.0 °C

0.6 %

Show Supplier Material materials with Shrinkage, transverse of 0.6 %

ISO 294-4, DAM

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Processing methods

Injection Molding