RADILON A LRV600W 333 BK

Alternative and trade names
PA66-GF60
Want to keep this datasheet? Save it now in your required format

Description

PA66 60% glass fibre reinforced injection moulding grade. Good flowability, heat stabilized. Black colour.

Suitable for parts requiring very high stiffness and high mechanical resistance, as in case of metal replacement applications. Good resistance to thermal ageing.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting StandardThickness

Density

1.7 g/cm³

Show Supplier Material materials with Density of 1.7 g/cm³

dry

ISO 1183

Moisture absorption

1 %

Show Supplier Material materials with Moisture absorption of 1 %

50% RH

ISO 62

2 mm

Water absorption

3.7 %

Show Supplier Material materials with Water absorption of 3.7 %

ISO 62

2 mm

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

21 GPa

Show Supplier Material materials with Elastic modulus of 21 GPa

dry

ISO 527-2/1A

1mm/min

Elongation

2 %

Show Supplier Material materials with Elongation of 2 %

dry

ISO 527-2/1A

5mm/min

Flexural modulus

20 GPa

Show Supplier Material materials with Flexural modulus of 20 GPa

dry

ISO 178

2mm/min

Flexural strength

400 MPa

Show Supplier Material materials with Flexural strength of 400 MPa

dry

ISO 178

2mm/min

Impact strength, Charpy notched

-30 °C

16 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m²

dry

ISO 179/1eA

23 °C

17 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 17 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

95 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m²

dry

ISO 179/1eU

23 °C

100 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m²

dry

ISO 179/1eU

Unlock all property charts

Tensile strength

260 MPa

Show Supplier Material materials with Tensile strength of 260 MPa

dry

ISO 527-2/1A

5mm/min

Thermal

PropertyValueThicknessTesting StandardPressureComment

Glow Wire Flammability Index

700 °C

Show Supplier Material materials with Glow Wire Flammability Index of 700 °C

2 mm

IEC 60695-2-12

Heat deflection temperature

260 °C

Show Supplier Material materials with Heat deflection temperature of 260 °C

ISO 75/2Af

2 MPa

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 11357-1/-3

10°C/min

Flammability

Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 | Class: HB ,method: UL 94, and thickness tested (mm): 0.8

Electrical

PropertyValueConditionTesting StandardComment

Surface resistivity

1e+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq

50%RH

IEC 60093

500V

1e+12 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq

dry

IEC 60093

500V

Volume resistivity

1e+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm

50%RH

IEC 60093

500V

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

dry

IEC 60093

500V

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Fillers

60% Glass Fiber

Processing methods

Injection Molding