General
Property | Value | Testing Standard |
---|---|---|
Density | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | ISO 1183 |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elastic modulus | 0.025 GPa Show Supplier Material materials with Elastic modulus of 0.025 GPa | ISO 527-2/1A | 1mm/min |
Elongation | 800 % Show Supplier Material materials with Elongation of 800 % | ISO 527-2/1A | 50mm/min | nominal |
Flexural modulus | 0.035 GPa Show Supplier Material materials with Flexural modulus of 0.035 GPa | ISO 178 | 2mm/min |
Flexural strength | 4 MPa Show Supplier Material materials with Flexural strength of 4 MPa | ISO 178 | 2mm/min |
Hardness, Shore D | 22 [-] Show Supplier Material materials with Hardness, Shore D of 22 [-] | ISO 7619-1 | 15s |
25 [-] Show Supplier Material materials with Hardness, Shore D of 25 [-] | ISO 7619-1 | inst. | |
Impact strength, Charpy notched | No Break at 23°C | ISO 179/1eA | |
Impact strength, Charpy unnotched | No Break at 23°C | ISO 179/1eU | |
Modulus at 10% elongation | 0.002 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.002 GPa | ISO 527-2/1A | |
Modulus at 100% elongation | 0.005 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.005 GPa | ISO 527-2/1A | |
Modulus at 300% elongation | 0.007 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.007 GPa | ISO 527-2/1A |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 175 °C Show Supplier Material materials with Melting point of 175 °C | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 11.5 g/10min Show Supplier Material materials with Melt mass-flow rate of 11.5 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |