General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Abrasion resistance | 19 mm³ Show Supplier Material materials with Abrasion resistance of 19 mm³ | ISO 4649 | |
Density | 1.15 g/cm³ Show Supplier Material materials with Density of 1.15 g/cm³ | ISO 1183 | |
Water absorption | 0.45 % Show Supplier Material materials with Water absorption of 0.45 % | ISO 62@1 | immersion at 23°C |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elastic modulus | 0.06 GPa Show Supplier Material materials with Elastic modulus of 0.06 GPa | ISO 527-2/1A | 1mm/min |
Elongation | 800 % Show Supplier Material materials with Elongation of 800 % | ISO 527-2/1A | 50mm/min | nominal |
Flexural modulus | 0.095 GPa Show Supplier Material materials with Flexural modulus of 0.095 GPa | ISO 178 | 2mm/min |
Flexural strength | 6 MPa Show Supplier Material materials with Flexural strength of 6 MPa | ISO 178 | 2mm/min |
Hardness, Shore D | 43 [-] Show Supplier Material materials with Hardness, Shore D of 43 [-] | ISO 7619-1 | 15s |
47 [-] Show Supplier Material materials with Hardness, Shore D of 47 [-] | ISO 7619-1 | inst. | |
Impact strength, Charpy notched | No Break at 23°C | ISO 179/1eA | |
Modulus at 10% elongation | 0.006 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.006 GPa | ISO 527-2/1A | |
Modulus at 100% elongation | 0.011 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.011 GPa | ISO 527-2/1A | |
Modulus at 300% elongation | 0.012 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.012 GPa | ISO 527-2/1A | |
Tear strength | 142 kN/m Show Supplier Material materials with Tear strength of 142 kN/m | ISO 34-1 |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Heat deflection temperature | 70 °C Show Supplier Material materials with Heat deflection temperature of 70 °C | ISO 75/2Bf | 0.45 MPa |
Melting point | 186 °C Show Supplier Material materials with Melting point of 186 °C | ISO 11357-1/-3 | 10°C/min |
Vicat softening temperature | 150 °C Show Supplier Material materials with Vicat softening temperature of 150 °C | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 34 g/10min Show Supplier Material materials with Melt mass-flow rate of 34 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |