General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Abrasion resistance | 39 mm³ Show Supplier Material materials with Abrasion resistance of 39 mm³ | ISO 4649 | |
Density | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | ISO 1183 | |
Water absorption | 0.1 % Show Supplier Material materials with Water absorption of 0.1 % | ISO 62@1 | immersion at 23°C |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 1.4 GPa Show Supplier Material materials with Elastic modulus of 1.4 GPa | ISO 527-2/1A | 1mm/min | |
Elongation | 350 % Show Supplier Material materials with Elongation of 350 % | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 15 % Show Supplier Material materials with Elongation at yield of 15 % | ISO 527-2/1A | 50mm/min | |
Flexural modulus | 1.3 GPa Show Supplier Material materials with Flexural modulus of 1.3 GPa | ISO 178 | 2mm/min | |
Flexural strength | 50 MPa Show Supplier Material materials with Flexural strength of 50 MPa | ISO 178 | 2mm/min | |
Hardness, Shore D | 69 [-] Show Supplier Material materials with Hardness, Shore D of 69 [-] | ISO 7619-1 | 15s | |
77 [-] Show Supplier Material materials with Hardness, Shore D of 77 [-] | ISO 7619-1 | inst. | ||
Impact strength, Charpy notched | 23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | ISO 179/1eA | |
Modulus at 10% elongation | 0.045 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.045 GPa | ISO 527-2/1A | ||
Modulus at 100% elongation | 0.032 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.032 GPa | ISO 527-2/1A | ||
Tear strength | 249 kN/m Show Supplier Material materials with Tear strength of 249 kN/m | ISO 34-1 | ||
Tensile strength | 29 MPa Show Supplier Material materials with Tensile strength of 29 MPa | ISO 527-2/1A | 5mm/min | |
Yield strength | 48 MPa Show Supplier Material materials with Yield strength of 48 MPa | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Heat deflection temperature | 60 °C Show Supplier Material materials with Heat deflection temperature of 60 °C | ISO 75/2Af | 1.80 MPa |
115 °C Show Supplier Material materials with Heat deflection temperature of 115 °C | ISO 75/2Bf | 0.45 MPa | |
Melting point | 219 °C Show Supplier Material materials with Melting point of 219 °C | ISO 11357-1/-3 | 10°C/min |
Vicat softening temperature | 210 °C Show Supplier Material materials with Vicat softening temperature of 210 °C | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 19 g/10min Show Supplier Material materials with Melt mass-flow rate of 19 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |