General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.21 g/cm³ Show Supplier Material materials with Density of 1.21 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 5.4 GPa Show Supplier Material materials with Elastic modulus of 5.4 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation | 3.8 % Show Supplier Material materials with Elongation of 3.8 % | dry | ISO 527-2/1A | 5mm/min | |
Flexural modulus | 4.4 GPa Show Supplier Material materials with Flexural modulus of 4.4 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 120 MPa Show Supplier Material materials with Flexural strength of 120 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 70 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | ISO 75/2Af | 1.80 MPa | ||
Melting point | 255 °C Show Supplier Material materials with Melting point of 255 °C | ISO 11357-1/-3 | 10°C/min | ||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 5 g/10min Show Supplier Material materials with Melt mass-flow rate of 5 g/10min | ISO 1133 | 275°C/10Kg |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 15% Glass Fiber | |
Processing methods | Injection Molding,Blow Molding |