General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.14 g/cm³ Show Supplier Material materials with Density of 1.14 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 8.9 % Show Supplier Material materials with Water absorption of 8.9 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 1.2 GPa Show Supplier Material materials with Elastic modulus of 1.2 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
3.0 GPa Show Supplier Material materials with Elastic modulus of 3.0 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 30 % Show Supplier Material materials with Elongation of 30 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
50 % Show Supplier Material materials with Elongation of 50 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | dry | ISO 527-2/1A | 50mm/min | |
30 % Show Supplier Material materials with Elongation at yield of 30 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Flexural modulus | 2.9 GPa Show Supplier Material materials with Flexural modulus of 2.9 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 110 MPa Show Supplier Material materials with Flexural strength of 110 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | No Break at 23°C | dry | ISO 179/1eU | ||
Yield strength | 55 MPa Show Supplier Material materials with Yield strength of 55 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
80 MPa Show Supplier Material materials with Yield strength of 80 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Thickness | Comment | |||
---|---|---|---|---|---|---|---|
Coefficient of thermal expansion | 8.5e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.5e-05 1/K | ISO 11359-1/-2 | 23°C-55°C | ||||
8.5e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.5e-05 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||||
Glow Wire Flammability Index | 800 °C Show Supplier Material materials with Glow Wire Flammability Index of 800 °C | IEC 60695-2-12 | 2 mm | ||||
Heat deflection temperature | 70 °C Show Supplier Material materials with Heat deflection temperature of 70 °C | ISO 75/2Af | 1.80 MPa | ||||
200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | ISO 75/2Bf | 0.45 MPa | |||||
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat softening temperature | 240 °C Show Supplier Material materials with Vicat softening temperature of 240 °C | ISO 306 | 50°C/h 50N | ||||
Flammability | Thickness tested (mm): 0.4 and 0.8, Class: V-2, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 1.2 % Show Supplier Material materials with Shrinkage of 1.2 % | 290/70/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | 290/70/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding |