General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2 % Show Supplier Material materials with Moisture absorption of 2 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 7.6 % Show Supplier Material materials with Water absorption of 7.6 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 1.2 GPa Show Supplier Material materials with Elastic modulus of 1.2 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.0 GPa Show Supplier Material materials with Elastic modulus of 2.0 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
50 % Show Supplier Material materials with Elongation of 50 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 15 % Show Supplier Material materials with Elongation at yield of 15 % | dry | ISO 527-2/1A | 50mm/min | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Flexural modulus | 2 GPa Show Supplier Material materials with Flexural modulus of 2 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 75 MPa Show Supplier Material materials with Flexural strength of 75 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | 50%RH | ISO 179/1eA | |
-30 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 72 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 72 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 90 kJ/m² | 50%RH | ISO 179/1eA | ||
Yield strength | 43 MPa Show Supplier Material materials with Yield strength of 43 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
55 MPa Show Supplier Material materials with Yield strength of 55 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 1.4 % Show Supplier Material materials with Shrinkage of 1.4 % | 290/70/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | 290/70/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding |