General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.06 g/cm³ Show Supplier Material materials with Density of 1.06 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 3 % Show Supplier Material materials with Water absorption of 3 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 2.3 GPa Show Supplier Material materials with Elastic modulus of 2.3 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation | 100 % Show Supplier Material materials with Elongation of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elongation at yield | 15 % Show Supplier Material materials with Elongation at yield of 15 % | dry | ISO 527-2/1A | 50mm/min | |
Flexural modulus | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 80 MPa Show Supplier Material materials with Flexural strength of 80 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 4.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | No Break at 23°C | dry | ISO 179/1eU | ||
Yield strength | 60 MPa Show Supplier Material materials with Yield strength of 60 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 215 °C Show Supplier Material materials with Melting point of 215 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Viscosity number | 100 cm³/gr Show Supplier Material materials with Viscosity number of 100 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Processing methods | Injection Molding |