General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.29 g/cm³ Show Supplier Material materials with Density of 1.29 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 1.9 % Show Supplier Material materials with Water absorption of 1.9 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 7.9 GPa Show Supplier Material materials with Elastic modulus of 7.9 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
8.8 GPa Show Supplier Material materials with Elastic modulus of 8.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 3.4 % Show Supplier Material materials with Elongation of 3.4 % | dry | ISO 527-2/1A | 5mm/min | |
4.1 % Show Supplier Material materials with Elongation of 4.1 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 6 GPa Show Supplier Material materials with Flexural modulus of 6 GPa | 50%RH | ISO 178 | 2mm/min | |
7.5 GPa Show Supplier Material materials with Flexural modulus of 7.5 GPa | dry | ISO 178 | 2mm/min | ||
Flexural strength | 205 MPa Show Supplier Material materials with Flexural strength of 205 MPa | 50%RH | ISO 178 | 2mm/min | |
240 MPa Show Supplier Material materials with Flexural strength of 240 MPa | dry | ISO 178 | 2mm/min | ||
Impact strength, Charpy notched | 23 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m² | dry | ISO 179/1eU | 23°C | |
80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Tensile strength | 130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
165 MPa Show Supplier Material materials with Tensile strength of 165 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coefficient of thermal expansion | 2e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-05 1/K | ISO 11359-1/-2 | 23°C-55°C |
0.00012 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.00012 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |
Melting point | 210 °C Show Supplier Material materials with Melting point of 210 °C | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.7 % Show Supplier Material materials with Shrinkage of 0.7 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, Drinking Water, RoHS 2011/65/UE | |
Color | Natural | |
Features | Hydrolysis Resistance | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |