General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.44 g/cm³ Show Supplier Material materials with Density of 1.44 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 13.1 GPa Show Supplier Material materials with Elastic modulus of 13.1 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation | 3.8 % Show Supplier Material materials with Elongation of 3.8 % | dry | ISO 527-2/1A | 5mm/min | |
Flexural modulus | 11.2 GPa Show Supplier Material materials with Flexural modulus of 11.2 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 280 MPa Show Supplier Material materials with Flexural strength of 280 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU | 23°C | |
Tensile strength | 185 MPa Show Supplier Material materials with Tensile strength of 185 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 212 °C Show Supplier Material materials with Melting point of 212 °C | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 45% Glass Fiber | |
Processing methods | Injection Molding |