General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.19 g/cm³ Show Supplier Material materials with Density of 1.19 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 6.5 % Show Supplier Material materials with Water absorption of 6.5 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 3.0 GPa Show Supplier Material materials with Elastic modulus of 3.0 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
4.8 GPa Show Supplier Material materials with Elastic modulus of 4.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 5 % Show Supplier Material materials with Elongation of 5 % | dry | ISO 527-2/1A | 5mm/min | |
14 % Show Supplier Material materials with Elongation of 14 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | 50%RH | ISO 178 | 2mm/min | |
4.3 GPa Show Supplier Material materials with Flexural modulus of 4.3 GPa | dry | ISO 178 | 2mm/min | ||
Flexural strength | 90 MPa Show Supplier Material materials with Flexural strength of 90 MPa | 50%RH | ISO 178 | 2mm/min | |
160 MPa Show Supplier Material materials with Flexural strength of 160 MPa | dry | ISO 178 | 2mm/min | ||
Impact strength, Charpy notched | 23 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | 67 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 67 kJ/m² | dry | ISO 179/1eU | 23°C | |
95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Tensile strength | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
102 MPa Show Supplier Material materials with Tensile strength of 102 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | 2 mm | IEC 60695-2-12 | ||||
Heat deflection temperature | 185 °C Show Supplier Material materials with Heat deflection temperature of 185 °C | ISO 75/2Af | 1.80 MPa | ||||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat softening temperature | 205 °C Show Supplier Material materials with Vicat softening temperature of 205 °C | ISO 306 | 1mm | ||||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Fillers | 13% Glass Fiber | |
Processing methods | Injection Molding |