General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.23 g/cm³ Show Supplier Material materials with Density of 1.23 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 8.5 % Show Supplier Material materials with Water absorption of 8.5 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 3.8 GPa Show Supplier Material materials with Elastic modulus of 3.8 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
5.7 GPa Show Supplier Material materials with Elastic modulus of 5.7 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 4.5 % Show Supplier Material materials with Elongation of 4.5 % | dry | ISO 527-2/1A | 5mm/min | |
12 % Show Supplier Material materials with Elongation of 12 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 4.9 GPa Show Supplier Material materials with Flexural modulus of 4.9 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 190 MPa Show Supplier Material materials with Flexural strength of 190 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 5.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | 40 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m² | dry | ISO 179/1eU | -30°C | |
50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry | ISO 179/1eU | 23°C | ||
70 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Tensile strength | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Thickness | Comment | |||
---|---|---|---|---|---|---|---|
Coefficient of thermal expansion | 3e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3e-05 1/K | ISO 11359-1/-2 | 23°C-55°C | ||||
7e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7e-05 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||||
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | IEC 60695-2-12 | 2 mm | ||||
Heat deflection temperature | 190 °C Show Supplier Material materials with Heat deflection temperature of 190 °C | ISO 75/2Af | 1.80 MPa | ||||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat softening temperature | 205 °C Show Supplier Material materials with Vicat softening temperature of 205 °C | ISO 306 | 50°C/h 50N | ||||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.1 % Show Supplier Material materials with Shrinkage of 1.1 % | 280/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Fillers | 15% Glass Fiber | |
Processing methods | Injection Molding |